Irabha ye-Liquid Butadiene Styrene (LSBR)
I-LSBR iyi-copolymer enesisindo esiphansi sama-molecule ye-butadiene ne-styrene enesisindo sama-molecule esingu-2000-10000. Ine-insulation kagesi enhle kakhulu kanye nezakhiwo zomzimba, futhi ivame ukusetshenziswa emikhakheni eminingi efana namabhodi wesekethe, izinamathiselo kanye nezinto zokuvala.
Uma kuqhathaniswa ne-polybutadiene ewuketshezi (LPB), i-LSBR inokushisa okuphezulu kokuguquka kwengilazi kanye nokumelana okungcono kokushisa nokuguguleka. Ukufaka i-LPB esikhundleni se-LSBR kungathuthukisa ukugeleza kwe-glue ngesikhathi sokucubungula amapuleti e-copper clad.
Ipakishwe ku-50kg/isigubhu, 170kg/isigubhu, Isikhathi sokugcina singunyaka owodwa.
Imiyalelo yokuphepha:
Indawo yokugcina kufanele ibe sendaweni epholile, eyomile futhi engenisa umoya. Isimo esihle kakhulu siphakathi kuka -20 ~ 38℃. Isikhathi sokuphila seshelufu sezinyanga ezingu-12, uma siphelelwa yisikhathi, singasetshenziswa uma sisezingeni elijwayelekile ngokuhlolwa kabusha. Lapho ukuthutha kufanele kugweme imvula, ukukhanya kwelanga. Ungaxubani ne-oxidizer enamandla.
| Into | I-LSBR-1 | I-LSBR-2 | I-LSBR-3 | I-LSBR-4 | I-LSBR-5 |
| Isisindo sama-molecule | 3000 | 3000 | 5000 | 5000 | 5000 |
| Okuqukethwe kwe-Styrene (mol %) | 8 - 12 | 15 - 20 | 8 - 12 | 15 - 20 | 20 - 25 |
| Okuqukethwe kwe-vinyl(%) | 80 - 90 | 20 - 30 | |||
| Ukuthamba(I-1965)45℃/113℉, Pa·s) | 60 | 300 | 150 | 500 | 60 |
| Okuguquguqukayo (%) | ≤2 | ||||
| Ukubukeka | Uketshezi olucwebezelayo olunombala okhanyayo | ||||